ÀÌ ¿¬±¸ÀÇ ¸ñÀûÀº 3D ÇÁ¸°Æà ·¹ÁøÀÇ ¿¬¸¶ ¹æ¹ý¿¡ µû¸¥ »öÁ¶ ¾ÈÁ¤¼º°ú Ç¥¸é Á¶µµ¸¦ ½Ã°£¿¡ µû¶ó ºñ±³ÇÏ´Â °ÍÀÌ´Ù. 3D ÇÁ¸°ÅÍ¿Í TC-80DP ·¹ÁøÀ» ÀÌ¿ëÇÏ¿© 3D ÇÁ¸°Æà ·¹Áø ½ÃÆíÀ»Á¦ÀÛÇÏ¿´°í, °¢ ½ÃÆíÀº ¿¬¸¶ÇÏÁö ¾ÊÀº ±º, Enhance¢ç±º, Sof-LexTM±ºÀ¸·Î ºÐ·ùµÇ¾ú´Ù. °¢±ºÀº ¿¬¸¶ Á÷ÈÄ ±âÁØÁ¡À» ÃøÁ¤ÇÏ°í, ´Ù½Ã Àΰø Ÿ¾×°ú ¿À·»Áö ÁÖ½º¿¡ ³ª´©¾î ħÀü½ÃŲ µÚ, ħÀü 1, 7, 30, 60ÀÏ¿¡ CIE L*a*b* °ªÀÇ »öÂ÷(¥ÄE*)¿Í °¢ ½ÃÁ¡ÀÇ Ç¥¸é Á¶µµ°¡ ÃøÁ¤µÇ¾ú´Ù.
¿¬±¸ °á°ú, 60ÀÏ Ä§Àü ÈÄ Àΰø Ÿ¾×¿¡¼­´Â À°¾ÈÀ¸·Î È®ÀÎ °¡´ÉÇÑ Á¤µµÀÇ »öÁ¶ º¯È­´Â ÀϾÁö ¾Ê¾ÒÀ¸³ª ¿À·»Áö ÁÖ½º¿¡¼­´Â À°¾ÈÀ¸·Î È®ÀÎ °¡´ÉÇÑ »öÁ¶ º¯È­°¡ ³ªÅ¸³µ°í, ¿ë¾×¿¡ µû¸¥ Â÷ÀÌ´Â À¯ÀǹÌÇß´Ù. Ç¥¸é Á¶µµ´Â Sof-LexTM±º¿¡¼­¸¸ ¿À·»Áö ÁÖ½º°¡ Àΰø Ÿ¾×º¸´Ù À¯ÀÇÇÏ°Ô ³ô¾Ò´Ù. ¿¬¸¶ ¹æ¹ý¿¡ µû¸¥ »öÁ¶ º¯È­ÀÇ Â÷ÀÌ´Â ¾ø¾úÀ¸³ª Ç¥¸é Á¶µµ´Â Sof-LexTM±ºÀÌ ¿¬¸¶ÇÏÁö ¾ÊÀº ±º°ú Enhance¢ç±ºº¸´Ù À¯ÀÇÇÏ°Ô ³·¾ÒÀ¸¸ç, ¸ðµç ±º¿¡¼­ Ä¡Å ħÂø ÀÓ°è Á¶µµº¸´Ù´Â ³ô¾ÒÁö¸¸, ÀÓ»óÀûÀ¸·Î Çã¿ë °¡´ÉÇÑ Á¤µµ¿´´Ù. À̹ø ¿¬±¸ °á°ú, À¯ÀüÄ¡ ÀüÀå°ü ¼öº¹À» À§ÇØ ¿µ±¸ ¼öº¹¿ë 3D ÇÁ¸°Æà ·¹Áø »ç¿ë ½Ã Âø»öÁ¦ ¼·Ãë¿¡ À¯ÀÇÇØ¾ß Çϸç, Sof- LexTM¸¦ ÀÌ¿ëÇÏ¿© ¿¬¸¶ÇÏ´Â °ÍÀÌ ±ÇÀåµÈ´Ù.

This study aimed to compare the color stability and surface roughness of three-dimensional (3D) printing resin according to polishing methods. 3D-printed resin specimens were fabricated at TC-80DP (Graphy, Seoul, Korea) with a stereolithography 3D printer, and the specimens were divided into three groups, each of which was not polished, was polished using Enhance¢ç, and was polished using a Sof-LexTM disc. The CIE L*a*b* value and the surface roughness of each group were measured and immersed in artificial saliva and orange juice after 0, 1, 7, 30, and 60 days, and the color difference (¥ÄE*) was calculated. As a result of the study, no noticeable color change was observed in artificial saliva, but a noticeable color change was demonstrated in orange juice after 60 days of immersion, and the difference was significant. In the Sof-LexTM group, surface roughness according to the solution was found to be significantly higher in the orange juice than that in artificial saliva. No significant difference in color change was found according to the polishing method, but surface roughness was significantly lower in the Sof-LexTM group than both that of the unpolished group and that of the Enhance¢ç group. Nevertheless, all groups exhibited clinically acceptable properties regardless of their higher surface roughness than the threshold for plaque accumulation. Overall, this study recommends utilizing Sof-LexTM for polishing 3D printing resin when used in primary anterior tooth coverage.

Å°¿öµå

3D printing; Resin; Color stability; Surface roughness; Polishing method

¿ø¹® ¹× ¸µÅ©¾Æ¿ô Á¤º¸

 

µîÀçÀú³Î Á¤º¸

KCI