Àá½Ã¸¸ ±â´Ù·Á ÁÖ¼¼¿ä. ·ÎµùÁßÀÔ´Ï´Ù.

±¤ÁßÇÕÇü ·¹ÁøÀÇ ÀüȯÀ² °áÁ¤À» À§ÇÑ 3°¡Áö ¹æ¹ýÀÇ ºñ±³

Comparison of three methods for determination of the degree of conversion in commercial light-cured composites: DSC and FTIR based on weight percent of methacrylate groups versus FTIR with an internal standard

´ëÇÑÄ¡°ú±âÀçÇÐȸÁö 2013³â 40±Ç 4È£ p.281 ~ 287
¿º¿ë¸®, ±ÇÅ¿±, ±è±³ÇÑ, ±è¿µ°æ,
¼Ò¼Ó »ó¼¼Á¤º¸
¿º¿ë¸® ( Yan Yong-Li ) - °æºÏ´ëÇб³ ´ëÇпø ÀÇ¿ë»ýü°øÇаú
±ÇÅ¿± ( Kwon Tae-Yub ) - °æºÏ´ëÇб³ Ä¡ÀÇÇÐÀü¹®´ëÇпø Ä¡°ú»ýüÀç·áÇб³½Ç
±è±³ÇÑ ( Kim Kho-Han ) - °æºÏ´ëÇб³ Ä¡ÀÇÇÐÀü¹®´ëÇпø Ä¡°ú»ýüÀç·áÇб³½Ç
±è¿µ°æ ( Kim Young-Kyung ) - °æºÏ´ëÇб³ Ä¡ÀÇÇÐÀü¹®´ëÇпø Ä¡°úº¸Á¸Çб³½Ç

Abstract

º» ½ÇÇèÀÇ ¸ñÀûÀº DSC¿Í FTIRÀ» ÅëÇØ °áÁ¤ÇÑ º¹ÇÕ ·¹ÁøÀÇ ÀüȯÀ²À» ºñ±³ÇÏ´Â °ÍÀÌ´Ù. ´Ù¼¸ °¡Áö ½ÃÆÇ ÁßÀÎ º¹ÇÕ ·¹ÁøÀ» »ç¿ëÇÏ¿´´Ù. FTIRÀ» ÀÌ¿ëÇÏ¿© ¿©·¯ ³óµµ·Î Èñ¼®½ÃŲ methyl methacrylate (MMA)ÀÇ °ËÁ¤°î¼±À» ±¸ÇÏ¿´´Ù. Weight percent of methacrylate groups (WPMG) ¹æ¹ýÀ» ÀÌ¿ëÇÏ¿© ·¹ÁøÀÇ ÁßÇÕ ÀüÈÄÀÇ WPMG º¯È­¸¦ °è»êÇÏ¿´´Ù. ¶ÇÇÑ DSC ¹æ¹ýÀ» ÀÌ¿ëÇÏ¿© ÀÌ·ÐÀûÀÎ ¹ß¿­°ª (exotherm)°ú ½ÇÇèÀûÀÎ ¹ß¿­°ªÀ» °áÁ¤ÇÏ¿´´Ù. ´Ù¼¸ °¡Áö º¹ÇÕ ·¹Áø¿¡ ´ëÇÏ¿© internal standard, WPMG, DSC ¹æ¹ýÀ» ÅëÇØ ÀüȯÀ²À» °è»êÇÏ¿´´Ù. Internal standard¿Í WPMG ¹æ¹ýÀ» »ç¿ëÇÑ °æ¿ì °¢ º¹ÇÕ ·¹Áø¿¡¼­ À¯ÀÇÇÑ Â÷ÀÌ°¡ °üÂûµÇÁö ¾Ê¾ÒÀ¸³ª (p>0.05), DSC ¹æ¹ýÀ» »ç¿ëÇÑ °æ¿ì À¯ÀÇÇÏ°Ô ³·Àº ÀüȯÀ² °ªÀÌ ¾ò¾îÁ³´Ù (p<0.05). FTIR·Î º¹ÇÕ ·¹ÁøÀÇ ÀüȯÀ²À» ÃøÁ¤ ½Ã internal standard°¡ Àû´çÇÏÁö ¾ÊÀº °æ¿ì WPMG ¹æ¹ýÀ» Àû¿ëÇÒ ¼ö ÀÖÀ» °ÍÀ¸·Î »ý°¢µÈ´Ù.

Å°¿öµå

Resin composite; Degree of conversion; DSC; FTIR spectroscopy