Abstract

º» ¿¬±¸´Â »ó¾ÆÁú Á¢ÂøÁ¦¿Í ·¹Áø ½Ã¸àÆ®ÀÇ ÀûÇÕ¼º ¿©ºÎ¸¦ ¾Ë¾Æº¸°íÀÚ ½ÃÇàÇÏ¿´´Ù. ¹ß°ÅÇÑ Á¦3´ë±¸Ä¡ÀÇ »ó¾ÆÁú Ç¥¸éÀ» ³ëÃâ½ÃŲ ÈÄ Tescera ATL º¹ÇÕ·¹Áø ½ÃÆíÀ» »ó¾ÆÁú Á¢ÂøÁ¦ [All Bond 2 (Bisco), Clearfil SE Bond (Kuraray), Adper Prompt L-POP (3M), One-Up Bond F (Tokuyama)]¿Í ·¹Áø½Ã¸àÆ® [Choice (Bisco), Panavia F (Kuraray), RelyX ARC (3M), Bistite II DC (Tokuyama)]·Î Á¢ÂøÇÏ°í ¹Ì¼¼ÀÎÀå °áÇÕ°­µµ ¹× ÁÖ»çÀüÀÚ Çö¹Ì°æ °üÂûÀ» ½ÃÇàÇÑ °á·ÐÀº ´ÙÀ½°ú °°´Ù. 1. Clearfil SE Bond¿Í All-Bond 2°¡ Prompt L-Pop°ú One-Up Bond F º¸´Ù ³ôÀº ¹Ì¼¼ÀÎÀå °áÇÕ°­µµ¸¦ º¸¿´´Ù(p<0.05). 2. Clearfil SE Bond¿Í All-Bond 2 »ç¿ë½Ã 1-step »ó¾ÆÁú Á¢ÂøÁ¦º¸´Ù È¥¼ºÃþÀÌ µÎ²®°í ·¹Áø tag°¡ ±æ¾ú´Ù.

This study was performed to investigate the compatibility between 4 dentin adhesives and 4 resin luting cements. Dentin adhesives used in this study were All-Bond 2 (Bisco Inc., Schaumbrug, IL, USA), Clearfil SE-Bond (Kuraray Medical Inc, Osaka, Japan), Prompt L-Pop (3M Dental Products, St. Paul, MN, USA), One-Up Bond F (Tokuyama corp., Tokyo, Japan) Resin luting cements used in this study were Choice (Bisco Inc., Schaumbrug, IL, USA), Panavia F (Kuraray Medical Inc, Osaka, Japan), RelyX ARC (3M Dental Products, St. Paul, MN, USA) Bistite II DC (Tokuyama corp., Tokyo, Japan). Combination of each dentin adhesive and corresponding resin cement was made to 16 experimental groups. Flat dentin surfaces was created on mid-coronal dentin of extracted mandibular third molars, then dentin surface was polished with 320-grit silicon carbide abrasive papers. Indirect resin composite block (Tescera, Bisco) was fabricated. Its surface for bonding to tooth was polished with silicon carbide abrasive papers Each dentin adhesive was treated on tooth surface and resin composite overlay were luted with each resin cement. Each bonded specimen was poured in epoxy resin and sectioned occluso-gingivally into 1.0mm thick slab, then further sectioned into $1.0{\times}1.0mm^2$ composite-dentin beams. Microtensile bond strength was tested at a crosshead speed of 1.0mm/min. The data were analysed by one-way ANOVA and Duncan¡¯¡¯s multiple comparison tests The results of this study were as follows, 2-step self-etching dentin adhesive which has additional bonding resin is more comparison than tests. self-etching dentin adhesive.

Å°¿öµå

ÀÚ°¡ºÎ½ÄÇü »ó¾ÆÁúÁ¢ÂøÁ¦;·¹Áø½Ã¸àÆ®;ÀûÇÕ¼º;¹Ì¼¼ÀÎÀå °áÇÕ°­µµ;È¥¼ºÃþ;º¹ÇÕ·¹Áø ½ÃÆí