Abstract

ÀÌ ¿¬±¸ÀÇ ¸ñÀûÀº ·¹Áø ÄÚÆÃµÈ Ç¥¸é°ú ·¹ÁøÀη¹ÀÌ »çÀÌÀÇ ÀÚ°¡-Á¢Âø ·¹Áø½Ã¸àÆ®¸¦ ÀÌ¿ëÇÑ °áÇÕ ½Ã Àӽð¡ºÀÁ¦¿¡ µû¸¥ ¹Ì¼¼ÀÎÀå°áÇÕ°­µµ¸¦ Æò°¡ÇÏ´Â °ÍÀ̾ú´Ù. Caviton(GC, Tokyo, Japan), Provifil(Promedica, Neumunster, Germany), Provifil(Promedica, Neumunster Germany) & petrolatum, and Eugenol-based cement, Tembond(Kerr, Orange. CA, USA) ÀÌ Àӽð¡ºÀÀç·Î »ç¿ëµÇ¾ú´Ù. Tescera(Bisco, Schamburg IL, USA) ·Î Á¦ÀÛÇÏ¿´°í ÀÚ°¡-Á¢Âø ·¹Áø½Ã¸àÆ®ÀÎ Rely X unicem (3M, St. Paul. Minn, USA) ¸¦ ÀÌ¿ëÇÏ¿© Á¢ÂøÇÏ¿´´Ù. ÀÌÈÄ ¹Ì¼¼ÀÎ Àå°áÇÕ°­µµ¸¦ ÃøÁ¤ÇÏ¿´°í one-way anova ¿Í Duncan test ¸¦ ÀÌ¿ëÇÏ¿© ºÐ¼®ÇÏ¿´´Ù.(p<0.05) Caviton ±ºÀÌ ´Ù¸¥ ±×·ì°ú ºñ±³ÇÏ¿© À¯ÀǼº ÀÖ´Â Â÷À̸¦ º¸¿©ÁÖ¾ú´Ù(p<0.05). Provifil, Provifil & petrolatum, Tembond ±º µîÀº »ó´ëÀûÀ¸·Î ³·Àº °ªÀ» º¸¿©ÁÖ¾ú´Ù.

The purpose of this research was to compare the microtensile bond strength of resin coated surface and resin inlay according temporary filling materials prior to applying self-adhesive resin cement. Caviton(GC, Japan), Provifil(Promedica, Neumunster, Germany), Provifil(Promedica, Neumunster, Germany) & petrolatum, and Eugenol-based cement, Tembond(Kerr, Orange CA, USA) were used as temporary filling materials. After fabrication of Tescera(Bisco, Schamburg IL, USA), it was bonded with a self-adhesive resin cement, Rely X unicem(3M, St. Paul. Minn, USA). After this procedure, the microtensile bond strength was measured and it was analyzed through one-way ANOVA and Duncan test(p<0.05). Caviton(GC, Tokyo, Japan) showed statistical difference except for the control(group I) and the saliva(group II)(p<0.05). Provifil(group IV), Provifil & petroneum(group V), Tembond(group VI) had lower microtensile bond strength.

Å°¿öµå

ÀúÁ¡µµ º¹ÇÕ·¹Áø;¹Ì¼¼°áÇÕÀÎÀå°­µµ;·¹Áø ÄÚÆøé
Low-viscosity composite resin;Microtensile bond strength;Resin-coating surface;Caviton;Tembond;Provifil